The glaze should be low in boron oxide,alkali
and other aggressive fluxes.
Excessive zircon in the glaze can cause the intensity of color not
satisfying,due to the over-opaqueness.
Do not grind or ball mill the colors but can stir into glaze with
a Jiffy Mixer.
SYG120/121/123
Included orange
Zr-Si-Cd-S-Se
Zircon
1250
SYG126
Included bright red
Zr-Si-Cd-S-Se
Zircon
1250
SYG127
Included dark red
Zr-Si-Cd-S-Se
Zircon
1250
These inclusion stains consist of Zirconium Silicate
incorporating Cadmium Sulphoselenide crystals, and are
manufactured in large batches by using a unique processing method.
Superior consistency and homogeneity of product is guaranteed.
These cadmium encapsulated stains offer great stability,as well as
compliance with safety and health requirements.